The concentration of Sb(III) and Sb(total) in an electroless nickel bath is determined by anodic stripping voltammetry (ASV). In c(HCl) = 0.6 mol/L only Sb(III) shows a signal. In w(HCl) = 10% the Sb(total) content is determined.